DAM/WIREMELT test1
Updated: Aug 23, 2019
Initial testing dam wire melt combination

issues
Pre firing
Dam put onto of a piece of kiln paper and lined with fibre paper. Fibre paper cut to shape and glass put on top (approximate colours to number 4 from the colour palette)
Post firing
Fibre paper stuck to edges, kiln paper fallen through so is fused in and has left a shadow on the surface as it cooled. Lots of big bubbles, lots of spikes. Not good.